Full Text Available
Note: Clicking the button above will open the full text document at the original institutional repository in a new window.
This dissertation presents the results of an investigation to develop a two-stage flotation process to produce: (i) a low-volume sulfide-rich concentrate that can be treated chemically or biologically or disposed of in a contained manner; (ii) a high-volume (low sulfur) benign tailings, with low ARD...
| Main Author: | |
|---|---|
| Other Authors: | |
| Format: | Thesis |
| Language: | English |
| Published: |
Centre for Bioprocess Engineering Research
2015
|
| Subjects: | |
| Tags: |
No Tags, Be the first to tag this record!
|
| Summary: | This dissertation presents the results of an investigation to develop a two-stage flotation process to produce: (i) a low-volume sulfide-rich concentrate that can be treated chemically or biologically or disposed of in a contained manner; (ii) a high-volume (low sulfur) benign tailings, with low ARD potential compared to conventional tailings; and (iii) a coal concentrate that has added value on account of its low sulfur and ash content. Success requires integration of flotation, aqueous chemistry and mineral bioleaching expertise. The approach adopted in this exploratory study entails coal flotation in the first stage, which takes advantage of its natural hydrophobicity. |
|---|