Determination of appropriate mix ratios for concrete grades using Nigerian Portland-limestone grades 32.5 and 42.5

The construction of buildings by incompetent craftsmen and the use of low quality building materials, including low quality concrete have been identified in the literature as two of the major reasons for the incessant collapse of building in Nigeria. The roadside craftsmen/artisans usually/generally...

Full description

Saved in:
Bibliographic Details
Format: Article
Published: 2015
Tags: Add Tag
No Tags, Be the first to tag this record!

MARC

LEADER 00000njm a2000000a 4500
001 oai:repository.ui.edu.ng:123456789/10350
042 |a dc 
720 |a Agbede O.A  |e author 
720 |a Ajagbe W.O  |e author 
260 |c 2015 
520 |a The construction of buildings by incompetent craftsmen and the use of low quality building materials, including low quality concrete have been identified in the literature as two of the major reasons for the incessant collapse of building in Nigeria. The roadside craftsmen/artisans usually/generally construct buildings using 1:2:4 cement-fine aggregate-large aggregate mix ratio irrespective of the cement strength class. In this paper, the investigation conducted to determine the appropriate concrete mix ratios required to produce Class 20/25 and Class 25/30 concretes commonly used for design of building structural members using the Portland-limestone cement grades 32.5 and 42.5 that are available in the Nigerian open market is presented. Investigation revealed that the cube compressive strength of 1:2:4 concrete produced with Portland-limestone cement grade 32.5 is less than the minimum 25MPa required for concrete Class 20/25 and a richer 1:1.5:3 concrete produced with Portland-limestone cement grade 32.5 may be needed to produce concrete Class 20/25. Investigation also revealed that Portland limestone cement grade 32.5 may not be suitable for the production of concrete class 25/30 with cube compressive strength of 30MPa as the cube compressive strength of 1:1:2 concrete produced with Portland-limestone cement grade 32.5 may not attain 30MPa. Concrete strength classes 20/25 and class 25/30 can be produced with Portland-limestone cement grade 42.5 using 
024 8 |a https://repository.ui.edu.ng/handle/123456789/10350 
245 0 0 |a Determination of appropriate mix ratios for concrete grades using Nigerian Portland-limestone grades 32.5 and 42.5